Zinc vs Aluminum vs Magnesium Anodes (2026 Guide)
Engineering selection matrix covering electrochemical potential, active life, cadmium-free aluminum performance, and mixed-water hazards.
1. Quick Water-Type Selection Matrix
| Alloy Code | Water Environment | Open-Circuit Potential | Key Engineering Advantage | Example SKUs |
|---|---|---|---|---|
| Zn (Zinc) | Saltwater only | -1.03 V (Ag/AgCl) | Traditional US Mil-Spec MIL-A-18001; heavy compact density | CMX03, CM6644537101Z |
| Al (Aluminum) | Salt & Brackish water | -1.10 V (Ag/AgCl) | Cadmium-free, ~50% longer service life, 50% lighter shipping weight | CMX03AL, CMY200350FLKITA |
| Mg (Magnesium) | Freshwater only | -1.50 V (Ag/AgCl) | Highest driving voltage required for low-conductivity freshwater | CMX03M, CM6644537101M |
2. Avoiding Two Expensive B2B Spec Mistakes
- Do not mix alloys on the same vessel underwater: Mixing zinc and magnesium on one drive causes uneven galvanic draw and accelerated wastage.
- Do not run zinc in brackish river estuaries: Zinc forms an insulating hydroxide crust in lower-salinity water, halting protection; specify Aluminum-Indium (Al models) instead.